    The cement is produced by grinding a mixture of additives (pozzolana) prescribed by standards (max. 20) with Portland cement clinker by addition of a certain amount of retarder (gypsum) and sets and gains strength after a certain time being mixed with water.

    Generally the product can be used in all places where portland cement is applicable. Hydration temperature is relatively lower than portland cement. It is appropriate to use in concrete works performed in aggresive areas where the content of sulphate or chloride ion is high.


    Physical properties
        SC Cement Standard Unit
      Initial Setting Time 157 min. 60 Minute
      Final Setting Time 185 -- Minute
      Increase in volume 1 max. 10 cm
      Specific Surface
    (Blaine)
    4450 -- cm2/g
      Bulk Density 890 -- g/l
      2 Days Strength 25 min. 20 N/mm2
      28 Days Strength 55  min./max. 42.5/62.5  N/mm2



    Chemical properties
        SC Cement Standard Unit
    SO3 3.4 max 3.5 %